Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 43.3 MPa | 6280 psi | ASTM D638 |
Teknor Apex APEX® RE 9016A Polyvinyl Chloride, Rigid Features: Good Weather Resistance; High Impact Resistance Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 43.30 MPa | 6280 psi | ASTM D638 |
Entec Hyrene® PSCRY 14 General Purpose Polystyrene Available in North America Features: General PurposeRoHS Compliant Form: Pellets Information provided by Entec |