Teknor Apex APEX® RE 9016A Polyvinyl Chloride, Rigid

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, High Impact , PVC, Rigid Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® RE 9016A Polyvinyl Chloride, Rigid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good Weather Resistance; High Impact Resistance Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
10 seconds; ASTM D2240
Tensile Strength at Break 43.3 MPa
6280 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Tensile Modulus 2.87 GPa
416 ksi
ASTM D638
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
Compression Molded; ASTM D256
Dart Drop Total Energy 70.5 J/cm

@Temperature 22.8 °C
0.132 ft-lb/mil

@Temperature 73.0 °F
Procedure A
Descriptive Properties Value Comments
Appearance Opaque