Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 42.4 MPa | 6150 psi | ASTM D638 |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |