Mechanical Properties Metric English Comments
Tensile Strength at Break 42.4 MPa
6150 psi
ASTM D638
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified
Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..