Polymer Property : Tensile Strength at Break = 6110 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.1 MPa
6110 psi
5.1 mm/min; ASTM D638
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Tensile Strength at Break 42.1 MPa
6110 psi
ASTM D412
Huntsman IROGRAN® D 64 P 4777 TPU-Polyester
Polyether-based grades for film and sheet applications that require excellent resistance to hydrolysis and microbial attack.Information provided by Alliance Polymers
Tensile Strength at Break 42.1 MPa
6110 psi
TD; ASTM D882
DuPont Surlyn® 1650SB
DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to ..