Polymer Property : Tensile Strength at Break = 5870 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.5 MPa
5870 psi
ASTM D638
IRPC Polimaxx Polene GA3750 High Density Polyethylene
CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS
Tensile Strength at Break 40.5 MPa
5870 psi
ASTM D638
IRPC Polimaxx Polene GA3750 High Density Polyethylene
CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS