Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 40.5 MPa | 5870 psi | ASTM D638 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Tensile Strength at Break | 40.5 MPa | 5870 psi | ASTM D638 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |