Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 558 MPa | 81000 psi | |
Shakespeare NX-1037 Nylon 6 Monofilament Low monomer for wet environments, flexible, resilient, resists compactionInformation provided by Shakespeare Company. |
|||
Tensile Strength at Break | 558 MPa | 81000 psi | |
Shakespeare WN-125 diameter 0.4 mm Nylon 66 Monofilament Paper Machine Clothing MonofilamentHigh molecular weightNylon 6,6Low modulusAbrasion resistanceLow shrinkageHeat stable Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | 558 MPa | 81000 psi | |
Shakespeare WN-250 diameter 0.2 mm Nylon 6 Monofilament Paper Machine Clothing MonofilamentNylon 6Moderate ModulusHigh shrinkage forceHigh shrinkage Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | 558 MPa | 81000 psi | |
Shakespeare WN-250 diameter 0.4 mm Nylon 6 Monofilament Paper Machine Clothing MonofilamentNylon 6Moderate ModulusHigh shrinkage forceHigh shrinkage Information provided by Shakespeare Company. |