Shakespeare WN-125 diameter 0.4 mm Nylon 66 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66 Fiber
Manufacturer Shakespeare Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare WN-125 diameter 0.4 mm Nylon 66 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Paper Machine Clothing MonofilamentHigh molecular weightNylon 6,6Low modulusAbrasion resistanceLow shrinkageHeat stable Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break 558 MPa
81000 psi
Elongation at Break 30 %
30 %
Elongation at Yield 13 %
13 %
at 3 g/D
Thermal Properties Metric English Comments
Shrinkage 3.00 %

@Temperature 175 °C
3.00 %

@Temperature 347 °F