Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 51.6 MPa | 7480 psi | 102% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 51.6 MPa | 7480 psi | ACMA Test #4 / DIN EN 843-1 |
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |