Mechanical Properties Metric English Comments
Tensile Strength at Break 5.31 MPa
770 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Strength at Break 5.31 MPa
770 psi
ASTM D412
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 5.31 MPa
770 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..