Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.31 MPa | 770 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2055 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 5.31 MPa | 770 psi | ASTM D412 |
Teknor Apex Telcar® TL-1522E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 5.31 MPa | 770 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |