Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.12 - 33.83 MPa | 2773 - 4907 psi | |
Taiwan PU Corporation PPG CPU-2095 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Tensile Strength at Break | 24.03 - 33.83 MPa | 3485 - 4907 psi | |
Taiwan PU Corporation PPG CPU-2172 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |