Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation PPG CPU-2095 Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation PPG CPU-2095 Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing.Information provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Viscosity 8000 - 15000 cP

@Temperature 40.0 °C
8000 - 15000 cP

@Temperature 104 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 93 - 97
93 - 97
Tensile Strength at Break 19.12 - 33.83 MPa
2773 - 4907 psi
Elongation at Break 360 - 460 %
360 - 460 %
Tear Strength 113 - 152 kN/m
644 - 868 pli
Processing Properties Metric English Comments
Processing Temperature 85.0 °C
185 °F
Working Temperature, Prepolymer
Mold Temperature 100 °C
212 °F
Pot Life 5.0 min
5.0 min
Descriptive Properties Value Comments
MOCA Temperature 110°C
NCO Content Max 6%
Min 5.6%
PHR of MOCA 16.7%