Polymer Property : Tensile Strength at Break = 464300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 3201 MPa
464300 psi
Hardwire 3x2 Cord
The 3x2 Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3x2 wire cord is made by twisting 5 individual wire together - three straight filam..