Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3201 MPa | 464300 psi | |
Hardwire 3x2 Cord The 3x2 Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3x2 wire cord is made by twisting 5 individual wire together - three straight filam.. |