Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 31.4 MPa | 4560 psi | ASTM D 638 |
Shakespeare Isocorâ„¢ HG20SC Nylon 612 Isocorâ„¢ HG20SC us a medium viscosity compounding grad PA-612 based nylon. This resin is specifically suited for applications requiring lower moisture regain and greater dimensional stability... |
|||
Tensile Strength at Break | 31.4 MPa | 4560 psi | ASTM D 638 |
Shakespeare Isocorâ„¢ HG26SI medium viscosity PA-612 Isocorâ„¢ HG26SI is a medium viscosity PA-612 based nylon. This resin is specifically suited for applications requiring low moisture regain and greater dimensional stability. Isocorâ„¢ HG2.. |