Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.06 MPa @Temperature 23.0 °C |
444 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Tensile Strength at Break | 3.06 MPa | 444 psi | ASTM D412 |
3M Scotchcast™ 2104 Electrical Insulating Resin Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical.. |