Polymer Property : Tensile Strength at Break = 4420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.5 MPa
4420 psi
Indium Corp. Indalloy 229 Lead Solder Alloy
Information Provided by Indium Corporation
Tensile Strength at Break 30.5 MPa
4420 psi
60% Ret.
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..