Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.83 MPa @Temperature 23.0 °C |
410 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Tensile Strength at Break | 2.83 MPa | 410 psi | ASTM D638 |
ExxonMobil OPTEMA™ TC 140 Molding, extrusion, compounding and adhesive resin
(discontinued **) OPTEMA TC 140 is a high flow, 21.5% methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compou.. |
|||
Tensile Strength at Break | 2.83 MPa @Time 1.21e+6 sec |
410 psi @Time 336 hour |
Standard cure |
3M AC-730 Class B-12 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Tensile Strength at Break | 2.83 MPa @Time 1.21e+6 sec |
410 psi @Time 336 hour |
Standard cure |
3M AC-730 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Tensile Strength at Break | 2.83 MPa @Time 1.21e+6 sec |
410 psi @Time 336 hour |
Standard cure |
3M AC-730 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Tensile Strength at Break | 2.83 MPa @Time 1.21e+6 sec |
410 psi @Time 336 hour |
Standard cure |
3M AC-730 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |