Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 2.83 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.83 MPa

@Temperature 23.0 °C
410 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Tensile Strength at Break 2.83 MPa
410 psi
ASTM D638
ExxonMobil OPTEMA™ TC 140 Molding, extrusion, compounding and adhesive resin  (discontinued **)
OPTEMA TC 140 is a high flow, 21.5% methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compou..
Tensile Strength at Break 2.83 MPa

@Time 1.21e+6 sec
410 psi

@Time 336 hour
Standard cure
3M AC-730 Class B-12 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Tensile Strength at Break 2.83 MPa

@Time 1.21e+6 sec
410 psi

@Time 336 hour
Standard cure
3M AC-730 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Tensile Strength at Break 2.83 MPa

@Time 1.21e+6 sec
410 psi

@Time 336 hour
Standard cure
3M AC-730 Class B-6 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Tensile Strength at Break 2.83 MPa

@Time 1.21e+6 sec
410 psi

@Time 336 hour
Standard cure
3M AC-730 Class B-1/2 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Copyright © lookpolymers.com All Rights Reserved