Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 26.0 - 28.0 MPa | 3770 - 4060 psi | ASTM D683 |
Loxim 821 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Tensile Strength at Break | 26.0 - 28.0 MPa | 3770 - 4060 psi | ASTM D683 |
Loxim 830 02C HB Polypropylene Compound, 30% Calcite Filled, Flame Retardant Information provided by Loxim Industries |
|||
Tensile Strength at Break | 26.0 - 28.0 MPa | 3770 - 4060 psi | ASTM D683 |
Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant Information provided by Loxim Industries |