Polymer Property : Tensile Strength at Break = 3830 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.4 MPa
3830 psi
50 mm/min; ASTM D638
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade
ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys..