Mechanical Properties Metric English Comments
Tensile Strength at Break 24.1 - 26.2 MPa
3500 - 3800 psi
ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo..