Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 251 MPa @Temperature -40.0 °C |
36400 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |
|||
Tensile Strength at Break | 251 MPa @Temperature -40.0 °C |
36400 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |