Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 24.5 MPa | 3550 psi | 50 mm/min; ISO 527 |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 50 mm/min; ISO 527 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 50 mm/min; ISO 527 |
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **) Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 500 mm/min; ASTM D638 |
Eastman M30033-P Voridian Polyethylene
(discontinued **) VORIDIAN M30033-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M30033-P has been found to exhibit good barrier properties, tempe.. |
|||
Tensile Strength at Break | 24.5 MPa @Thickness 2.00 mm |
3550 psi @Thickness 0.0787 in |
50mm/min; ASTM D638 |
LG Chemical KEYFLEX BT 5035D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | ASTM D638 |
LG Chemical LC100 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear applicationApplication: Polymer modification, Shoe sole, Film coex.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HM5001 High density polyethylene HM5001 is a high density polyethylene for yarn extrusion. HM5001 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2aApplic.. |
|||
Tensile Strength at Break | >= 24.5 MPa | >= 3550 psi | |
Sibur Nitrilast-40M Nitrile-Butadiene Rubber (NBR) N 3809 DN 108. For production of oil-benzene resistant articles for the automobile, aviation and rubber technical industries. Rubbers on the base of Nitrilast possess good oil-benzene resistance. .. |
|||
Tensile Strength at Break | >= 24.5 MPa | >= 3550 psi | |
Sibur SKS-30 ARKM-15 2nd Group Oil-Filled Styrene-Butadiene Rubber SBR 1705. For use in the tire industry for production of tire thread and other parts for tires, in the rubber technical industry for production of a wide assortment of rubber technical articles, an.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | ISO R 527 |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | ASTM D638 |
Teknor Apex APEX® 80873 Polyvinyl Chloride, Semi-Rigid Notes: 105°C Insulation; RoHS Compliant Features: Semi-rigid Uses: Insulation; Automotive Electronics Agency Ratings: UL 1063; UL 1581; UL 83; SAE J1128 Forms: Pellets Wire Types: THHN; THW; TW; .. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 553 Flame Retardant Polystyrene Characteristics High flow properties Good balance of toughness and rigidity Available in any color Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, electric.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 564 Flame Retardant Polystyrene Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Processing MoldingApplications Large size T.V. Cabinets VCR cabinets Electrical boxes, ele.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP6415 High Gloss High Impact Polystyrene Characteristics Very good gloss with the retention of ESCR properties Good toughness Also available in various color shades Processing Injection moldingApplications Refrigerator end caps Refriger.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 500mm/min; ASTM D638 |
Westlake MC3033 High Density Polyethylene Coating Westlake MC3033 is a high density polyethylene designed for extrusion coating and lamination applications. MC3033 provides improved barrier properties, temperature resistance, stress crack resistanc.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | ISO 527-1/-2 |
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 731 9920 High Impact Polystyrene Characteristics Speciality grade containing silicon oil to provide wear resistance and high opacity jet black color Easy flowing grade Processing Injection moldingApplications Camera parts Photogr.. |
|||
Tensile Strength at Break | 24.5 MPa | 3550 psi | ISO 527-1/-2 |
DSM Arnitel® PM581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |