Polymer Property : Tensile Strength at Break = 34500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 238 MPa
34500 psi
ASTM D638
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced
Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch..
Tensile Strength at Break 238 MPa
34500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength at Break 238 MPa
34500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RC00A PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RC00A is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive
Tensile Strength at Break 238 MPa
34500 psi
ASTM D638
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific)
LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.