Mechanical Properties Metric English Comments
Tensile Strength at Break 345 MPa
50000 psi
Shakespeare MX-305 HDPE Monofilament
Generally good chemical resistance. Good biological resistance.Information provided by Shakespeare Company.
Tensile Strength at Break 345 MPa
50000 psi
Annealed
California Fine Wire Nickel 220 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 345 MPa
50000 psi
Annealed
California Fine Wire Nickel 271 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 345 MPa
50000 psi
Annealed
California Fine Wire Nickel 272 Super Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 345 MPa
50000 psi
Annealed
California Fine Wire Nickel 5900 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 345 MPa
50000 psi
Annealed
California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 345 MPa
50000 psi
Annealed
California Fine Wire Nickel Alloy 99
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Tensile Strength at Break 345 MPa
50000 psi
Annealed
California Fine Wire Nickel Alloy 99 Nickel Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.