Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 31.0 - 34.6 MPa | 4500 - 5020 psi | ASTM D638M |
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features.. |