Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 31.9 MPa | 4630 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 6503 High Impact Polystyrene Characteristics High Impact Available in various colors Easy flow High stiffness Processing Injection moldingApplications Computer cabinet, printer body, business machine housing etc. Material St.. |
|||
Tensile Strength at Break | 31.9 MPa | 4630 psi | ASTM D638 |
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |
|||
Tensile Strength at Break | 31.9 MPa | 4630 psi | ASTM D3759 |
3M 97065 General Purpose Aluminum Foil Tape 60 lb. moisture stable liner. Good for die-cut applications.Information provided by 3M |