Polymer Property : Tensile Strength at Break = 31.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.00 MPa
4496 psi
ASTM D638 ISO 527-2
DuPont Surlyn® PC2000  (discontinued **)
DuPont™ Surlyn® PC2000 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA c..