Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.79 MPa
550 psi
Elastic; ASTM D412
Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection Molding Features:Gloss, LowInformation provided by Multibase
Tensile Strength at Break 3.79 MPa

@Temperature 23.0 °C
550 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro..
Tensile Strength at Break 3.79 MPa

@Temperature 23.0 °C
550 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV..
Tensile Strength at Break 3.79 - 4.14 MPa
550 - 600 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ HTE 1102 Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne
Tensile Strength at Break 3.79 MPa

@Temperature 23.0 °C
550 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over..
Tensile Strength at Break 3.79 MPa
550 psi
ASTM D412
Teknor Apex Monprene® MP-1870A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 3.79 MPa
550 psi
ASTM D412
Teknor Apex Telcar® TL-2625A Thermoplastic Elastomer
Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext..
Tensile Strength at Break 3.79 MPa
550 psi
ASTM D412
Teknor Apex Telcar® TL-2635C Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Tensile Strength at Break 3.79 MPa
550 psi
ASTM D412
Teknor Apex Telcar® TL-2069B Thermoplastic Elastomer
Uses: Caps; Food Packaging; Liners Pellets Processing Method: Extrusion; Injection Molding; Press Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmIn..
Tensile Strength at Break 3.79 MPa
550 psi
ASTM D638
ExxonMobil Escorene™ UL 7741 Ethylene Vinyl Acetate Copolymer
Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends..