Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.79 MPa | 550 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection Molding Features:Gloss, LowInformation provided by Multibase |
|||
Tensile Strength at Break | 3.79 MPa @Temperature 23.0 °C |
550 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro.. |
|||
Tensile Strength at Break | 3.79 MPa @Temperature 23.0 °C |
550 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Tensile Strength at Break | 3.79 - 4.14 MPa | 550 - 600 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ HTE 1102 Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Tensile Strength at Break | 3.79 MPa @Temperature 23.0 °C |
550 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Tensile Strength at Break | 3.79 MPa | 550 psi | ASTM D412 |
Teknor Apex Monprene® MP-1870A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.79 MPa | 550 psi | ASTM D412 |
Teknor Apex Telcar® TL-2625A Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext.. |
|||
Tensile Strength at Break | 3.79 MPa | 550 psi | ASTM D412 |
Teknor Apex Telcar® TL-2635C Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Tensile Strength at Break | 3.79 MPa | 550 psi | ASTM D412 |
Teknor Apex Telcar® TL-2069B Thermoplastic Elastomer Uses: Caps; Food Packaging; Liners Pellets Processing Method: Extrusion; Injection Molding; Press Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmIn.. |
|||
Tensile Strength at Break | 3.79 MPa | 550 psi | ASTM D638 |
ExxonMobil Escorene™ UL 7741 Ethylene Vinyl Acetate Copolymer Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends.. |