Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.72 MPa | 540 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 281-45MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength at Break | 3.72 MPa | 540 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Tensile Strength at Break | 3.72 MPa | 540 psi | 275°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 8291-85PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Tensile Strength at Break | 3.72 MPa @Temperature 23.0 °C |
540 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Tensile Strength at Break | 3.72 MPa | 540 psi | Heat Aged 24 hours at 600F |
Malvern Minerals Sliastic 437 with 50% Novacite® Daper Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |