Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft combinations are required. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.Information provided by Advanced Elastomer Systems
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Thickness 2.00 mm
70

@Thickness 0.0787 in
ISO 868
Tensile Strength at Break 3.72 MPa
540 psi
Across Flow; ASTM D412
Tensile Strength, Ultimate 2.55 MPa
370 psi
Across Flow; ASTM D412
Elongation at Break 380 %
380 %
Across Flow; ASTM D412
Tear Strength 17.7 kN/m
101 pli
73°F, Die C; ASTM D624
Compression Set 39 %
39 %
ASTM D395; ASTM D395
79 %
79 %
257°F, 70 hr; ASTM D395
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Descriptive Properties Value Comments
Color Natural Color
Form Pellets