Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 296 MPa | 43000 psi | Lengthwise; ASTM D638 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Tensile Strength at Break | 296 MPa | 43000 psi | |
Shakespeare HPA-14 diameter 0.7 mm PPS Monofilament Paper Machine Clothing MonofilamentChemical resistantHigh service temperatureNon-hydrolyzingWarp yarnHigh shrinkage Information provided by Shakespeare Company. |