Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 250 Silver Based Cadmium Free Filler Metal Characteristics:Braze 250 is an intermediate temperature silver brazing alloy with a long (325EF/180EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting constitu.. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 300 Silver Based Cadmium Free Filler Metal Characteristics: Braze 300 is an intermediate temperature silver brazing alloy with a fairly long (160EF/70EC) melting range. This long melting range is helpful when wide gap joints are brazed and .. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 541 Silver Based Cadmium Free Filler Metal Characteristics:Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting .. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 716 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp.. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 716 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp.. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into.. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt BRAZE 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc.. |
|||
Tensile Strength at Break | 241 - 276 MPa | 35000 - 40000 psi | Nickel-Silver butt joint |
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin.. |
|||
Tensile Strength at Break | 207 - 276 MPa | 30000 - 40000 psi | Brass butt joint |
Lucas-Milhaupt BRAZE 560 Characteristics:Braze 560 is a low temperature, free-flowing brazing filler metal with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through it.. |