Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 271 MPa | 39300 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 LNP* THERMOCOMP* RC006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength at Break | 271 MPa | 39300 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 (Asia Pacific) LNP* Thermocomp* RC006 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength at Break | 271 MPa | 39300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC006H PA 66 LNP THERMOCOMP* RC006H is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare |