Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.16 - 26.97 MPa | 2489 - 3912 psi | |
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |