Tensile Strength at Break 17.06 MPa
2475 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2179 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2179 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..