Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.06 MPa | 2475 psi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2179 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2179 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |