Mechanical Properties Metric English Comments
Tensile Strength at Break 1.59 MPa

@Time 7200 sec
231 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-1000 TPE
Product Description: StarGrip GP 25-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery..
Tensile Strength at Break 1.59 MPa

@Temperature 60.0 °C
231 psi

@Temperature 140 °F
JRF-14 days
3M AC-350 Class A-1 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
Tensile Strength at Break 1.59 MPa

@Temperature 60.0 °C
231 psi

@Temperature 140 °F
JRF-14 days
3M AC-350 Class A-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
Tensile Strength at Break 1.59 MPa

@Temperature 60.0 °C
231 psi

@Temperature 140 °F
JRF-14 days
3M AC-350 Class A-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
Tensile Strength at Break 1.59 MPa

@Temperature 336 °C
231 psi

@Temperature 637 °F
MIL-PRF-81733 AND AS5127A
3M AC-736 B-2 Aerospace Sealant
3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an ..
Tensile Strength at Break 1.59 MPa

@Time 605000 sec
231 psi

@Time 168 hour
180°F (82°C) and then tested at 75°F (24°C)
3M Weatherban™ 606NF Acrylic Sealant
3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M..