Mechanical Properties Metric English Comments
Tensile Strength at Break 1.59 MPa

@Time 7200 sec
231 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-1000 TPE
Product Description: StarGrip GP 25-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery..
Tensile Strength at Break 1.59 MPa
230 psi
ASTM D638
ExxonMobil Escorene® UL 7710 Adhesive Application Resin
Escorene Ultra UL 7710 is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt ..
Tensile Strength at Break 1.59 MPa
230 psi
ASTM D638
ExxonMobil Escorene® UL 7710E Adhesive Application Resin
Escorene Ultra UL 7710E is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt..
Tensile Strength at Break 1.59 MPa

@Temperature 60.0 °C
231 psi

@Temperature 140 °F
JRF-14 days
3M AC-350 Class A-1 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
Tensile Strength at Break 1.59 MPa

@Temperature 60.0 °C
231 psi

@Temperature 140 °F
JRF-14 days
3M AC-350 Class A-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
Tensile Strength at Break 1.59 MPa

@Temperature 60.0 °C
231 psi

@Temperature 140 °F
JRF-14 days
3M AC-350 Class A-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have..
Tensile Strength at Break 1.59 MPa

@Temperature 336 °C
231 psi

@Temperature 637 °F
MIL-PRF-81733 AND AS5127A
3M AC-736 B-2 Aerospace Sealant
3M Aerospace Sealant AC-736 B-2 is a non-chromate corrosion inhabiting sealants, fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealant. These Sealants act as an ..
Tensile Strength at Break 1.59 MPa

@Time 605000 sec
231 psi

@Time 168 hour
180°F (82°C) and then tested at 75°F (24°C)
3M Weatherban™ 606NF Acrylic Sealant
3M™ Weatherban™ Acrylic Sealant 606NF is a bright, white, premium quality, water-based paintable sealant.Features:Water-basedPaintableWeather resistantConstruction, maintenance repair operation (M..