Polymer Property : Tensile Strength at Break = 23.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.159 MPa
23.0 psi
Abatron AboSeal 6-6™ Heavy-Duty Epoxy Expansion Joint Sealant
AboSeal 6-6™ is a 2-part epoxy with exceptional bond strength and flexibility. It is available in duel barrel cartridges. It can be applied to interior or exterior concrete, wood, metal, and compos..