Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.159 MPa | 23.0 psi | |
Abatron AboSeal 6-6™ Heavy-Duty Epoxy Expansion Joint Sealant AboSeal 6-6™ is a 2-part epoxy with exceptional bond strength and flexibility. It is available in duel barrel cartridges. It can be applied to interior or exterior concrete, wood, metal, and compos.. |