Mechanical Properties Metric English Comments
Tensile Strength at Break 15.4 MPa
2240 psi
ASTM D638
Teknor Apex APEX® 327 Polyvinyl Chloride, Flexible
Notes: 60°C Insulation; RoHS Compliant Uses: Flexible Cord Insulation; Flexible Cord JacketingForms: Pellets Wire Types: SJT; SPT-1; SPT-2; SPT-3; SRDT; ST; SVT Agency Ratings: UL 1581; UL 62 Pro..
Tensile Strength at Break 15.4 MPa
2240 psi
ASTM D638
Teknor Apex APEX® 6500-75 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
Tensile Strength at Break 15.4 MPa
2240 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5620Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5620Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..
Tensile Strength at Break 15.4 MPa
2240 psi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5621 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5621 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
Tensile Strength at Break 15.5 MPa
2240 psi
ASTM D3759
3M Tartan™ 8934 Utility Filament Tape
Tartan™ Utility Filament Tape 8934 is a glass filament reinforced tape for light duty strapping, bundling and reinforcing. It has a synthetic rubber resin adhesive with good adhesion to most fiberb..