Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1290 MPa | 187000 psi | Stress relieved |
California Fine Wire Alloy 436 Platinum/Tungsten Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 1290 MPa | 187000 psi | Stress relieved |
California Fine Wire Alloy 436L Precious Metal Alloy All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonInsulatedInformation provided by California Fine Wire. |