Polymer Property : Tensile Strength at Break = 1849.7 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.753 MPa
1849.7 psi
JIS-K-6723
Denka LCS Z1070 Thermoplastic Elastomer, Extrusion grade (general)
"DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r..
Tensile Strength at Break 12.753 MPa
1849.7 psi
JIS-K-6723
Denka REOMER G G3010 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Tensile Strength at Break 12.753 MPa
1849.7 psi
JIS-K-6723
Denka VINYKON S210075 PVC, S grade for transparent extrusion molding
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Tensile Strength at Break 12.753 MPa
1849.7 psi
JIS-K-6723
Denka LCS Z6060 Thermoplastic Elastomer, Injection Molding Grade (general)
"DENKA LCS" combines low hardness with a rubber-like texture, having a low permanent compressive distortion/permanent elongation, and is a thermoplastic elastomer that closely resembles vulcanized r..