Mechanical Properties Metric English Comments
Tensile Strength at Break 12.59 MPa
1826 psi
AVG; ASTM D412 Method A
Seals Eastern 5722 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.
Tensile Strength at Break 12.59 MPa
1826 psi
Change in tensile strength in air after 168 hours at 248°F; ASTM D573
Teknor Apex Telcar® TL-94-T1422A-100 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Tensile Strength at Break >= 12.59 MPa
>= 1826 psi
ASTM D412 Method A
Seals Eastern 5404 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.