Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.59 MPa | 1826 psi | AVG; ASTM D412 Method A |
Seals Eastern 5722 Fluorocarbon-Elastomer Formulated Viton®. General service.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 12.59 MPa | 1826 psi | Change in tensile strength in air after 168 hours at 248°F; ASTM D573 |
Teknor Apex Telcar® TL-94-T1422A-100 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Strength at Break | >= 12.59 MPa | >= 1826 psi | ASTM D412 Method A |
Seals Eastern 5404 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |